cond-mat/soft IB-arxiv-2606.24674-tpd-tsub-063-096tg measured

Vapor-deposited TPD glasses transform via fronts whose velocity varies over an order of magnitude for TSubstrate from 0.63 to 0.96 Tg.

Active Evidence state is recorded explicitly and may be revised by a later event.

Observed quantities

Tsub_low_over_Tg 0.63 · Tsub_high_over_Tg 0.96

01

Primary source

  1. arxiv · 2606.24674 · v1 · abstract
Title
Thermal stability of vapor-deposited stable glasses of an organic semiconductor
Authors
Diane M. Walters, Ranko Richert, M. D. Ediger
Version
v1
Check
Support quote found word for word in the arXiv abstract v1, 2026-10-08
Supporting quote from the source
prepared with substrate temperatures (TSubstrate) from 0.63 to 0.96 Tg, at many different annealing temperatures. We observe that the front velocity varies by over an order of magnitude with TSubstrate

02

Boundary of this block

No additional public limitation was recorded.

03

Connections

Outgoing

No outgoing public edges.

Incoming