  "oags": "0.2",
  "status": "alpha",
  "entry": {
    "id": "IB-arxiv-2606.24674-tpd-tsub-063-096tg",
    "type": "evidence",
    "claim": "Vapor-deposited TPD glasses transform via fronts whose velocity varies over an order of magnitude for TSubstrate from 0.63 to 0.96 Tg.",
    "evidence_grade": "E3",
    "state": "active",
    "primary_source_ref": [
      {
        "kind": "arxiv",
        "id": "2606.24674",
        "version": "v1",
        "url": "https://arxiv.org/abs/2606.24674",
        "locator": "abstract"
      }
    ],
    "quantities": {
      "Tsub_low_over_Tg": 0.63,
      "Tsub_high_over_Tg": 0.96
    },
    "declared_loss": null,
    "source_title": "Thermal stability of vapor-deposited stable glasses of an organic semiconductor",
    "authors": [
      "Diane M. Walters",
      "Ranko Richert",
      "M. D. Ediger"
    ],
    "result_origin": "measured",
    "support_quote": "prepared with substrate temperatures (TSubstrate) from 0.63 to 0.96 Tg, at many different annealing temperatures. We observe that the front velocity varies by over an order of magnitude with TSubstrate",
    "source_version": "v1",
    "abstract_check": {
      "version": "v1",
      "date": "2026-10-08",
      "quote_verbatim": true
    },
    "domain_v2": "cond-mat/soft"
  },
  "expand": [],
  "incoming": [],
  "links": [],
  "declared_losses": [
    "Public evidence-graph projection: internal analytic/theory edges and private provenance are withheld by design.",
    "Alpha: some primary-source refs await precise citation verification."
  ],
  "generated": "2026-10-08"
}